Skip to main content
. 2023 Aug 7;13(34):23745–23753. doi: 10.1039/d3ra04111e

Summary of synthetic conditions and assembled productsa.

Product formula Metal(ii) precursor ALb M2+/linker/AL/NaOH molar ratio Dimensi-onality
[Cu22-mia)2(phen)2(H2O)2]·2H2O (1) CuCl2·2H2O Phen 1/1/1/2 0D
[Mn(μ3-mia)(phen)]n (2) MnCl2·4H2O Phen 1/1/1/2 1D
[Co(μ2-mia)(2,2′-bipy)(H2O)]n·nH2O (3) CoCl2·6H2O 2,2′-Bipy 1/1/1/2 1D
[Co(μ3-mia)(μ2-4,4′-bipy)]n·nH2O (4) CoCl2·6H2O 4,4′-Bipy 1/1/1/2 2D
[Co(μ3-mia)(py)2]n (5) CoCl2·6H2O py 1/1/31/— 1D
[Cd(μ2-mia)(py)(H2O)2]n·nH2On (6) CdCl2·H2O py 1/1/31/— 1D
a

Hydrothermal synthesis: stainless steel reactor (25 mL volume; Teflon-lined), MCl2 (0.2 mmol), H2O (10 mL), 3 days at 160 °C, 10 °C h−1 cooling rate.

b

AL, N-donor auxiliary ligand. The oxidation state of the metals in compounds 1–5 was determined by the values of magnetic moment (Fig. S3 and Table S3).