Figure 12

The different laser processes were evaluated for their impact on the damage morphology on the sharp angle side of the microhole. The horizontal axis represents different scanning speeds: 80, 160, 240, and 320 mm/s, while the vertical axis represents laser powers of 12 W, 18 W, 24 W, and 30 W. Subfigure (ap) show the cross sections of the acute angle side scanning electron microscope at different scanning speeds and laser powers.