Figure 5.

Figure 5

(a) SEM image of CrMoNbTiZr before potentiodynamic polarization test. (b) Microstructure after corrosion in Hanks. (c) Microstructure after corrosion in PBS. Corresponding EDX analyses of the microstructural images of (ac) are shown in (df), respectively.