Bulk Si engineering for the advanced SiMP anode. (a) Schematic for the reliable structure of graphene cage-encapsulated SiMP after cycling. (b) In situ TEM time-lapse images of graphene cage-encapsulated SiMP during lithiation. Reproduced with permission from ref (48). Copyright 2016 Springer Nature. (c) Graphical representation of the operation of the PR-PAA binder to dissipate the stress during repeated volume changes of SiMPs. Reproduced with permission from ref (53). Copyright 2017 American Association for the Advancement of Science. (d) Schematic illustration of an integrated binder-conductive material system through functionalization. (e) Lithiation limited cycling of the bare SiMP anode and constructed SiMP anode at 0.5 C with state-of-charge (SOC) control to 50%.