Table 3.
Concentrations and crystallographic parameters of cellulose p-MNP samples subjected to extreme washing. Results were obtained by XRF and XRD.
| Samples | XRF (ppm and retention %) |
XRD |
|||||
|---|---|---|---|---|---|---|---|
| Ag | Cu | 1 0 | 110 | 200 | % CIr | ||
| p-AgNP | 905.1 ± 40.2 | – | dHKl (nm) | 0.612 | 0.546 | 0.391 | 80.7 |
| 90.14 | L (nm) | 4.407 | 5.840 | 5.214 | |||
| p-CuNP | – | 418.2 ± 42.7 | dHKl (nm) | 0.614 | 0.549 | 0.392 | 81.7 |
| 5.74 | L (nm) | 4.634 | 6.167 | 5.061 | |||
| p-Ag/CuNP | 781.3 ± 37.5 | 3328 ± 142 | dHKl (nm) | 0.615 | 0.548 | 0.391 | 82.9 |
| 96.81 | 30.25 | L (nm) | 4.758 | 5.518 | 5.158 | ||