Skip to main content
. 2023 Jul 10;15(33):39625–39635. doi: 10.1021/acsami.3c05306

Figure 6.

Figure 6

2D GIWAXS patterns for films on ZnO, shown as square root (intensity) to better clarify weaker features. Spin-coated (a) PM6, (b) DTY6, (c) PM6:DTY6 blend, (e) spray-coated PM6:DTY6 blend using optimum air-knife delay time. (d) 1D linecuts for blends and components. (f) 1D linecuts comparing out-of-plane intensity for spin- and spray-coated blends.