Skip to main content
. 2023 Aug 18;15(16):3450. doi: 10.3390/polym15163450

Table 1.

The thickness of the electrodeposited and spin-coated PANI thin films.

Electrodeposited Spin Coated
Sample Thickness (nm) Sample Thickness (nm)
J5T300 25.8 ± 9.9 SC2000 8.8 ± 1.0
J5T600 62.9 ± 8.7 SC1000 11.0 ± 1.1
J5T1200 121.5 ± 27.9 SC500 13.2 ± 1.1