Skip to main content
. 2023 Aug 22;16(17):5747. doi: 10.3390/ma16175747

Figure 8.

Figure 8

The inverse pole figure maps of the coatings’ surface after heat treatment at 900 °C for 10 h, histograms of the grain size distribution, and distribution histograms of the boundary misorientation angle for the EHEA (ac) and YHf-EHEA (df).