Figure 7.

Figure 7

SEM and EDS analysis of the fracture of the sample after the shear strength test. (a) SEM image of the HTOA rubber layer; (b) holes (yellow arrows) and cracks (red dashed circles) of the HTOA matrix; (c) EDS analysis at the red dot.