Skip to main content
. 2023 Aug 23;16(17):5769. doi: 10.3390/ma16175769

Figure 8.

Figure 8

Crack morphology and particle chemical phase diagram caused by NCM phase transition. (a) SEM cross-sectional crack morphology of LiNi0.89Mn0.1Mo0.01O2 particles after 1000 cycles in the voltage range of 3.0–4.2V [37]; (b) SEM cross-sectional crack morphology of LiNi0.88Mn0.1Mo0.02O2 particles after the first cycle [38]; (c) chemical phase diagrams of oxidation and reduction phases in LiNi0.8Co0.15A10.05O2 [36].