(a) View of a partial cross-section of an apparatus suitable for carrying out the teachings of the invention; (b) Enlarged view of the substrate transport system utilized in the apparatus of (a). In a vacuum chamber “6”, a high voltage is applied by the generator “36” to an electrical wire “44” connected to a flexible contact strip “88” in contact with the supply spool “52” while the ground is imposed via “42” and “90” to the other supply spool “54”. Two flexible and metal substrates “66”, “68” are unwound from supply spools “52”, “54” and pass along convergent paths to guide rollers “58”, “60”. [2] (c) SEM micrograph showing the etched surface of a Nylon fiber after 5 min of plasma treatment using the process of Anderson in 1960 (reproduced with permission) [3] Copyright 2004 AIP Publishing. (d) Effect of corona duration on nylon peel strength and polypropylene wettability, adapted from [11].