Skip to main content
. 2023 Aug 1;38(3):438–454. doi: 10.1177/08853282231190908

Figure 1.

Figure 1.

(a) Compressive strength of magnesium oxychloride cements with different PLRs (n = 10). (b)–(e) Images of magnesium oxychloride cements 24 h after setting at 37°C and 100% humidity in silicone molds. (b)–(d) PLR 1 g mL−1, (e) left mold: PLR 0.9 g mL−1, right mold: PLR 1.1 g mL−1.