Skip to main content
. 2023 Sep 19;16(18):6280. doi: 10.3390/ma16186280

Figure 10.

Figure 10

Adjusted mass change of 2nd generation FeCrAl alloys exposed to BWR-HWC (290 °C, 62 wppb DH) with fitted curves [69].