Skip to main content
. 2023 Sep 7;23(18):7732. doi: 10.3390/s23187732

Figure 8.

Figure 8

Cyclic voltammograms measured in 0.50 M H2SO4 within the potential range of 0.5 V to 1.5 V vs. Ag|AgCl at a scan rate of 50 mVs1 using bare GCE, MWCNT/Nafion-modified GCE (a), and TiO2/MWCNT/Nafion-modified GCE (b).