Turbidimetric analysis to follow DMPC liposomes solubilization using SSS-L30 and SSS-L36 copolymers at SSS:DMPC ratio of 1:1 (w/w). The O.D. was measured for samples under shaking at two different temperatures, 25 °C (A) and 37 °C (B). The labels L30 and L36 indicate DMPC liposomes solubilized by SSS-L30 and SSS-L36, respectively.