Skip to main content
. 2023 Sep 26;16(19):6406. doi: 10.3390/ma16196406

Figure 6.

Figure 6

The microstructures when the DMLS laser power is 180 W: (a) DMLS areas macro-morphology; (b,c) Microscopic morphology of the upper layer of the packaging area; (df) DMLS areas with microscopic defects.