Skip to main content
. 2023 Oct 16;13:17589. doi: 10.1038/s41598-023-44078-7

Figure 5.

Figure 5

Melt phase content determined by thermodynamic modelling. (a) After decarbonation (1100 °C), maximum silicate formation (1350 °C), and maximum clinkering (1450 °C) temperatures. (b) Phase evolution between 1250 and 1450 °C.