Figure 7.

Figure 7

Parameters for predicting sample melting below the clinkering temperature or collapse during cooling. (a) Shape of the samples after the fusibility test up to 1450 °C followed by cooling to 200 °C. (b) Relation between the iron content in the melt phase amount at 1450 °C by thermodynamic modelling. Validation of risk zones based on self-pulverising and Portland clinkers from the literature23,31,7075.