Table 3. Effect of Mo Doping on Grain Size and Roughness of V2O5 Thin Filmsa.

Sample Grain size (nm) Roughness (nm) Areal Capacitance (mF/cm2)
Pure V2O5 28 6 56
2% of Mo 30 9 66
4% of Mo 56 12 83
6% of Mo 63 10 52
a

Reproduced with permission from Prakash et al.103 Copyright 2016 ELSEVIER Materials Today: Proceedings.