Skip to main content
. 2023 Oct 24;23:789. doi: 10.1186/s12903-023-03515-9

Fig. 2.

Fig. 2

Mean color differences (∆E) of the tested resin composites after 84 days of immersion in Coffee and after repolishing. (A) Hand polished surface. (B) Machine polished surface. Values exceeding the dotted line indicate clinical unacceptability (∆E ≥ 3.3)