Fig. 4. Temporal evolution of SEI formation on lithium metal in EC + 1.2 M LiPF6 electrolyte.

Fig. 4

a Resulting species distribution in kMC box at selected times and b development of SEI thickness over time. Energy values comprise the case for EC reduction in the presence of Li+. Source data are provided as a Source Data file.