Skip to main content
. 2023 Oct 13;17(20):20434–20444. doi: 10.1021/acsnano.3c06879

Figure 4.

Figure 4

Evolution of the SEI layer with increasing number of cycles: (a) time series of ADF-STEM images showing the evolution of the SEI at the glassy-carbon electrode; (b–d) first, second, third, and fourth CVs, respectively, obtained from an operando ec liquid cell STEM experiment showing charge–discharge from GC electrode in LiPF6/EC/EMC liquid electrolyte at a flow rate of 2.5 μL/min.