Skip to main content
. 2023 Oct 30;15(44):50962–50972. doi: 10.1021/acsami.3c13584

Figure 5.

Figure 5

Representative traces from DMA showing no measurable shape recovery of samples with no GO (Figure 4A,B) but shape recovery with maximum strain changes of 1.5 and 6% of samples containing 0.3% GO (Figure 4C) and 2% GO (Figure 4D), respectively. (A) pure tBA-BA, (B) tBA-BA with PCL fibers with 0% GO, (C) tBA-BA with PCL fibers with 0.3% GO, and (D) tBA-BA with PCL fibers with 2% GO. tBA-BA (tert-butyl acrylate-butyl acrylate), GO (methacrylated graphene oxide), and PCL (poly(ε-caprolactone)).