Microtome workflow

(A) Soak the block in Mollifex followed by (B) ice water.

(C) Cut sections.

(D) The section is floated on a warm water bath until smooth and then (E) placed on a glass slide.

(F) Sections are allowed to dry upright at 18°C–22°C.