Skip to main content
. 2023 Oct 27;15(11):2542. doi: 10.3390/pharmaceutics15112542

Table 2.

Yield in spray drying process of 30% DL ritonavir with used polymers.

Polymer Yield in SD Process 1
PVA 3-82 54%
PVA 4-88 28%
Grafted copolymer 12%
PVP K30 35%
HPMC-AS 1%

1 The yield is calculated from the powder obtained in the product vessel in relation to the weighed-in mass for the preparation.