Skip to main content
. 2023 Nov 15;9(11):e22435. doi: 10.1016/j.heliyon.2023.e22435

Table 1.

Results of quantitative XRD analysisa of the obtained coatings.

Oxide
Layer
Phase, wt%
MgO MgAl2O4 Amorphous
PEO(1 kHz) 58.21 31.35 10.44
PEO(1 kHz) + n-SiO2 58.66 26.54 14.8
a

The estimated error is less than 5 % (by factor wRp in the Jana 2006 software).