Skip to main content
. 2023 Dec 5;23:967. doi: 10.1186/s12903-023-03711-7

Table 3.

Comparison of debonding forces between the study groups

Resin nanoceramic Group (n = 10) Lithium disilicate Group (n = 10) Test (P)
Mean ± SD 284.30 ± 26.44 253.30 ± 33.26

2.307

(0.033*)

95% CI for mean 265.39, 303.21 229.50, 277.10
Median (IQR) 283.50 (50.00) 247.00 (62.00)

*Statistically significant difference at P ≤ .05, 95% CI: Confidence Interval