. 2023 Nov 17;17(23):23955–23964. doi: 10.1021/acsnano.3c08534

Figure 8.

Figure 8

CO2 consumption for La0.43Ca0.37Ni0.06Ti0.94O3−δ before and after MW reduction treatments, namely, 1 and 5 exsolution cycles. Those two treatments were also compared to an in situ thermal exsolution (400 °C, 1 h under 5% H2/Ar flow) and with nonexsolved LCTN. All tests were carried out at 400 °C and GHSV = 13971 h–1.