Table 1. Average Intercalated atm % Determined by XPSa.
Hf 4f | Ti 2p | Zr 3d | |
---|---|---|---|
Bi2Se3 | 0.6(1) | 3.0(1) | 2.7(1) |
MoO3 | 2.1(1) | 0.2(1) | 0.8(1) |
nano-MoO3 | 1.1(1) | 12.2(1) | 1.3(1) |
GeS | 3.2(1) | 0.2(1) | 1.3(1) |
Si2Te3 | 1.6(1) | 3.0(1) | 0.7(1) |
nano is hydrothermally grown MoO3..