Skip to main content
. 2023 Dec 12;13(24):3120. doi: 10.3390/nano13243120

Figure 4.

Figure 4

UV-vis DRS of Au9-MPTMS@Na-LTA (0.75 ± 0.01 wt% Au) (a) before and after calcination under static air at different temperatures of 200, 300, and 400 °C and (b) after ozonolysis at different temperatures of 25, 150, 200, and 300 °C. (c) UV-vis DRS of Au9-MPTMS@Na-LTA with 0.75 ± 0.01 and 1.11 ± 0.02 wt% Au after ozonolysis at 200 °C.