Skip to main content
. 2023 Jul 21;14(1):208–222. doi: 10.1007/s13346-023-01393-w

Fig. 5.

Fig. 5

A Images of the slide and seal MAP-box, which was manufactured by FDM 3D-printing. B Surface of designed MAP-box using 50 × and 100 × magnification. C OCT images of MAP-box from different perspectives: top, side and bottom. D Moisture content of silica inside the designed MAP-box in open and closed system after exposed under 40 °C and 75% relative humidity at 1, 2 and 7 days (means + SD, n = 3). E Representative image for water contact angle measurement of the MAP-box surface. F Water contact angle measurement of MAP-box surface (means + SD, n = 3)