Pore parameters of 3D printing SrTCP scaffolds with different Sr-doping amounts.

Pre-set pore size/μm Actual pore size/μm Porosity/% Pore connectivity/%
β-TCP 400 381.92 ± 17.66 62.77 ± 4.26 100 ± 0.24
Sr5TCP 400 386.64 ± 24.10 63.69 ± 5.69 99.8 ± 0.38
Sr10 TCP 400 380.64 ± 9.25 64.78 ± 3.97 99.9 ± 0.27
Sr20 TCP 400 381.18 ± 16.43 62.74 ± 4.59 100 ± 0.49