Skip to main content
. 2023 Dec 16;12(1):178–191. doi: 10.1021/acssuschemeng.3c05296

Figure 6.

Figure 6

Depolymerization of PS90 using a 25 mL stainless steel reactor, eight 10 mm stainless steel balls, and 1 g of PS90 milled cl. for 40 min; (a) yield of styrene and benzaldehyde (two most abundant products) vs milling frequency using eight 10 mm diameter balls, (b) corresponding MWs for experiments in (a), and (c) yield of styrene and benzaldehyde vs ball mass, milling conducted at 30 Hz using 1 ball.