Figure 8.

Figure 8

Styrene yield (y axis) as a function of MW reduction (x axis) for milling at different frequencies, with both quantities normalized by number of chains counted after milling using number-average MW. Milling time (40 min), number (8) and size (10 mm) of balls, and mass of PS90 (1 g) kept constant across all experiments.