FTIR spectra: (a) initial Miscanthus cellulose (C0) after 2 h hydrolysis (C2), 8 h hydrolysis (C8), and 24 h hydrolysis (C24); and (b) CN from original cellulose (CN0), after 2 h hydrolysis (CN2), 8 h hydrolysis (CN8), and 24 h hydrolysis (CN24).