Table 2.
Sample | Temperature Range (°C)/Weight Loss (%) | Temperature of DTG Peak (°C) | ||||||
---|---|---|---|---|---|---|---|---|
I | II | III | IV | I | II | III | IV | |
3EPET-CuO | 292–482 | - | - | - | 409 | - | - | - |
EPET | 289–480 | - | - | - | 405 | - | - | - |
PVC-3CuO | 238–313/5.5 | 313–401/3.5 | 401–540/13.2 | 540–692/29 | 281 | 365 | 494 | 653 |
PVC | 203–371/65.3 | 371–536/28.9 | - | - | 288 | 454 | - | - |
9EPET-1PVC-3CuO | 242–328/4.3 | 328–439/22.5 | 439–636/18.3 | - | 279 | 392 | 554 | - |