Skip to main content
. 2024 Jan 11;15:479. doi: 10.1038/s41467-024-44728-y

Fig. 5. Retention and fatigue.

Fig. 5

a Retention and b fatigue tests in BPBO/BLFO/BPBO and SRO/BLFO/SRO heterostructures I after different temperature treatments. High-temperature BLFO heterostructure II deposited at 700 °C is also shown for comparison.