Table 1. Comparison of the Electrochemical Oxidation of AR Using La2YCrO6/HLNTs/GCE with Other Materials.

electrode material method pH linear range (μM) LOD (NM) references
TiO2/ErGO DPV 7 0.3–800 50 (43)
F-nanodiamond@SiO2@TiO2 DPV 3 0.01–8.65 1.22 (44)
SHU/PCFE LSV 4 0.01–2 0.36 (45)
LaOX-TiOX/CPE SWV 2.5   90 (46)
Mn3O4@C/SPM DPV   0.1–1748.4 0.3 (47)
La2YCrO6/HLNTs/GCE LSV 7 10–120 8.99 present work