Skip to main content
. 2024 Jan 18;14:1559. doi: 10.1038/s41598-024-52196-z

Table 5.

Resist pull-out ultimate bearing capacity of steel bars after each round of grouting with different calcium source concentrations (unit: N).

Number of grouting cycles The calcium source concentration is 0.5 mol/L The calcium source concentration is 1.0 mol/L The calcium source concentration is 2.0 mol/L
3 230.32 289.14 311.23
4 389.11 434.03 576.02
5 530.37 687.76 575.83
6 703.23 687.23
7 703.35

Due to the small amount of calcium carbonate generated in the first 2 rounds of grouting, their anchoring ability to the steel bar was insufficient, and the value could not be recorded.