Table 3. Residual Weight Percentage of Pure and Toughened Foams at Various Temperaturesa.
| residual weight % |
Tmax at 200–400 °C | Tmax at 400–800 °C | |||
|---|---|---|---|---|---|
| 400 °C | 600 °C | 800 °C | |||
| PF | 79.05 | 56.43 | 40.83 | 268 | 453 |
| PF-Li | 80.87 | 58.86 | 43.38 | 269 | 442 |
| PF-SS | 81.53 | 58.52 | 44.06 | 267 | 458 |
| PF-NC | 78.83 | 56.82 | 43.38 | 270 | 439 |
| PF-U | 81.14 | 58.52 | 44.44 | 281 | 461 |
Tmax—maximum degradation temperature, Residual weight—mass left in the sample.