. 2023 Dec 7;11(5):2307329. doi: 10.1002/advs.202307329

Figure 2.

Figure 2

In vitro degradation behavior of Zn‐2Mg scaffolds in Hank's solution: a) SEM images and EDS elemental analysis of the surface of the scaffold after 90 days of immersion, b) weight loss analysis of scaffolds (n = 3, *p < 0.05), c,d) compressive strength and elastic modulus after degradation (n = 3).