Table 2.
Crystal growth velocities (m/s) computed as described in Methods for the GeTe slab confined by the TiTe2-like capping layers (GeTe/TiTe2-like SL) for the bulk models (see text) with a thick (28 layers, Bulk28) molten region in contact with a crystalline slab and from homogeneous crystal nucleation and growth (Bulkhomo). At 700 and 750 K no crystal nucleation occurs in the bulk over the time scale of several ns.
| Temperature (K) | GeTe/TiTe2-like SL | Bulk28 | Bulkhomo |
|---|---|---|---|
| (m/s) | |||
| 500 | 0.1 | 0.5 | 0.7 |
| 550 | 0.4 | 1.3 | 1.4 |
| 600 | 0.9 | 3.9 | 2.4 |
| 650 | 1.6 | 4.0 | 4.5 |
| 700 | 1.7 | 3.7 | – |
| 750 | 2.3 | 3.4 | – |