Table 5. Tm of PE1 Nanocomposites Obtained by DSC after SSA Procedurea.
| PE1/ZrP-g-MPE11/5 | |||||
|---|---|---|---|---|---|
| Tm (°C) | Ts (°C) | ||||
| sample | 129.0 | 124.0 | 119.0 | 114.0 | 109.0 |
| PE1 | 135.9 | 124.6 | 119.2 | 114.1 | 109.2 |
| ZrP-g-MPE11/5 | 136.2 | 126.0 | 120.9 | 114.9 | 109.9 |
| PE1/ZrP-g-MPE11/5 | 135.7 | 125.1 | 120.1 | 114.6 | 109.6 |
| PE1/ZrP-g-MPE22/1 | |||||
|---|---|---|---|---|---|
| Tm (°C) | Ts (°C) | ||||
| sample | 128.5 | 123.5 | 118.5 | 113.5 | 108.5 |
| PE1 | 135.6 | 123.8 | 118.6 | 113.8 | 109.8 |
| ZrP-g-MPE22/1 | 136.1 | 126.0 | 120.3 | 114.3 | 109.1 |
| PE1/ZrP-g-MPE22/1 | 135.9 | 124.9 | 119.7 | 114.3 | 109.1 |
| PE1/ZrP-g-MPE32/1 | |||||
|---|---|---|---|---|---|
| Tm (°C) | Ts (°C) | ||||
| sample | 128.5 | 123.5 | 118.5 | 113.5 | 108.5 |
| PE1 | 135.6 | 123.8 | 118.6 | 113.8 | 109.8 |
| ZrP-g-MPE32/1 | 131.9 | 125.7 | 119.9 | 114.4 | 109.3 |
| PE1/ZrP-g-MPE32/1 | 137.5 and 132.6 | 125.1 | 119.7 | 114.1 | 109.0 |
First five fractionation temperatures and their corresponding Tm are shown.