Table 6. Tm of PE2 Nanocomposites Obtained by DSC after the SSA Procedurea.
| PE2/ZrP-g-MPE11/5 | |||||
|---|---|---|---|---|---|
| Tm (°C) | Ts (°C) | ||||
| sample | 129.0 | 124.0 | 119.0 | 114.0 | 109.0 |
| PE2 | 131.5 | 125.5 | 119.5 | 114.1 | 109.1 |
| ZrP-g-MPE11/5 | 135.5 | 126.2 | 120.6 | 114.9 | 109.8 |
| PE2/ZrP-g-MPE11/5 | 133.8 | 126.0 | 120.2 | 114.5 | 109.6 |
| PE2/ZrP-g-MPE22/1 | |||||
|---|---|---|---|---|---|
| Tm (°C) | Ts (°C) | ||||
| sample | 128.0 | 123.0 | 118.0 | 113.0 | 108.0 |
| PE2 | 131.8 | 124.8 | 118.4 | 113.3 | 108.3 |
| ZrP-g-MPE22/1 | 136.1 | 125.5 | 120.0 | 114.4 | 109.1 |
| PE2/ZrP-g-MPE22/1 | 133.5 | 125.1 | 119.3 | 114.0 | 108.9 |
| PE2/ZrP-g-MPE32/1 | |||||
|---|---|---|---|---|---|
| Tm (°C) | Ts (°C) | ||||
| sample | 128.0 | 123.0 | 118.0 | 113.0 | 108.0 |
| PE2 | 131.8 | 124.8 | 118.4 | 113.3 | 108.3 |
| ZrP-g-MPE32/1 | 131.4 | 125.5 | 119.9 | 114.1 | 108.6 |
| PE2/ZrP-g-MPE32/1 | 131.6 | 125.2 | 119.0 | 114.1 | 108.6 |
First five fractionation temperatures and their corresponding Tm are shown.