(a) Percent graft yield (GY%) of AN + AA binary mixture onto cellulose, monomer concentration = 10 v%, time = 60 min, [KMnO4] = 0.05 mol/L, M:L ratio = 1:100, temperature = 70 °C, [citric acid] = 0.02 mol/L. (b) Percent graft yield (GY%) of AN + Sty binary mixture onto cellulose, monomer concentration = 10 v%, time = 60 min, [KMnO4] = 0.05 mol/L, M:L ratio = 1:100, temperature = 70 °C, [citric acid] = 0.02 mol/L.