Skip to main content
. 2024 Feb 13;15(2):43. doi: 10.3390/jfb15020043

Figure 3.

Figure 3

FTIR spectra of the samples obtained after attaching chrysin on Fe3O4@PEG and Fe3O4@chitosan in different ratios: (A) Fe3O4@PEG250 with a 1:0.5 PEG-chrysin ratio; (B) Fe3O4@PEG500 with a 1:1 PEG-chrysin ratio; (C) Fe3O4@PEG1000 with a 1:2 PEG-chrysin ratio; (D) Fe3O4@Chitosan250 with a 1:0.5 chitosan-chrysin ratio; (E) Fe3O4@Chitosan500 with a 1:1 chitosan-chrysin ratio; (F) Fe3O4@Chitosan1000 with a 1:2 chitosan-chrysin ratio. The characteristic peaks in the spectra indicate that PEG and chitosan-coated magnetite NPs were successfully synthesized, and the chrysin drug was loaded into them.