Skip to main content
. 2024 Feb 7;17(4):794. doi: 10.3390/ma17040794

Figure 6.

Figure 6

EPMA mapping on the near-surface of the P–HIP Ti–48Al–3Nb–1.5Ta alloy after exposure to different conditions, and the red squares in the column two show the detected areas.