Skip to main content
. 2024 Feb 7;17(4):794. doi: 10.3390/ma17040794

Figure 15.

Figure 15

SEM images of the fracture surfaces after exposure at 800 °C for 1000 h: (a) Low magnification; (b) High magnification.