The effect of electrolysis temperature on electrodeposition reaction.
| No. | Cathode material and diameter (mm) | Temperature (°C) | Electrolysis time (h) | Uranium concentration in molten salt (U3O8 : molten salt) | Electrolysis voltage (V) | Recovery efficiency of UO2 (%) |
|---|---|---|---|---|---|---|
| 7 | Graphite Φ 5 | 600 | 5 | 1 : 100 | −1.2 | 94 |
| 5 | Graphite Φ 5 | 650 | 5 | 1 : 100 | −1.2 | 95 |
| 8 | Graphite Φ 5 | 700 | 5 | 1 : 100 | −1.2 | 93 |