Table 3.
CIE chromaticity coordinates of glass samples annealed at 320 °C and 650 °C (the codes match as shown in Fig. 8).
| Sample | Code | CIE coordinates | |
|---|---|---|---|
| x | y | ||
| 0.5% Er2O3 glass at 320 °C | A | 0.240 | 0.474 |
| 1% Er2O3 glass at 320 °C | B | 0.263 | 0.460 |
| 0.5% Er2O3 glass at 650 °C | C | 0.267 | 0.450 |
| 1% Er2O3 glass at 650 °C | D | 0.260 | 0.426 |
| 0.5% Tb2O3 glass at 320 °C | E | 0.294 | 0.450 |
| 1% Tb2O3 glass at 320 °C | F | 0.279 | 0.473 |
| 0.5% Tb2O3 glass at 650 °C | G | 0.300 | 0.501 |
| 0.5%Tb2O3 glass at 650 °C | H | 0.298 | 0.543 |